[1] Individual elements flux may vary upto 15%.
[2] ULP models are tested under following conditions: 1500 PPM feed water, 25 °C, 15% recovery.
[3] SW models are tested under following conditions: 32000 PPM feed water, 25 °C, 8% recovery.
[4] BW models are tested under following conditions: 2000 PPM feed water, 25 °C, 15% recovery.
[5] LP models are tested under following conditions: 2000 PPM feed water, 25 °C, 15% recovery.